Casting RFQ Checklist: What to Send a Foundry

Send a foundry a dimensioned drawing with the 3D model, the material specification, the quantities, and every test and document you require. Add what the part does, how it ships, and how you want the quote laid out.

This checklist assumes a ferrous sand casting going out for quotation, either a new part or one moving from another foundry.

  • Drawing package: dimensioned drawing, 3D model, revision, part number, casting weight.
  • Tolerances: general grade with its document, critical dimensions, datums.
  • Material: specification and grade, or required properties, plus test bar and heat treatment condition.
  • Quantities: annual requirement, schedule, batch size, program length, samples.
  • Machining: marked surfaces, allowance, who machines.
  • Tooling: details of existing patterns, or a request to price new ones.
  • Process: named only if you have a reason to fix it.
  • Inspection: NDT, mechanical, hardness and pressure tests, each with its acceptance level.
  • Documents: certificates and reports, listed by name.
  • Finish and coating: comparator level, coating specification.
  • Application: what the part does, service conditions, failure history.
  • Delivery: address, date, delivery term, packaging.
  • Quote format: what to price separately, exceptions, validity date, surcharge basis.

What Goes in the Drawing Package

Send a dimensioned 2D drawing and the 3D model, with the same revision on both, and say which file governs if they disagree. The ISO casting tolerance standard, ISO 8062-3, does not apply to a 3D model used without indicated dimensions, so a model sent alone leaves the as-cast tolerance undefined.

Add the part number, a description and the rough casting weight, actual or estimated.

The drawing itself can take several forms, and they are not equally good:

  • Combined drawing: one drawing shows the cast part in solid lines and the machined dimensions in broken lines. Many foundries prefer this form.
  • Machine drawing plus casting drawing: the same information on two drawings, so keep their revisions matched.
  • Machine drawing only: the foundry adds the finish stock, which leaves more room for misunderstanding.
  • Casting drawing only: the weakest choice.

Use one drawing for one part, and do not cover several similar parts by changing a bore size or a length. Mark highly stressed areas, and mark where any numbers or letters should be cast on.

Leave draft and fillet radii to the foundry unless a mating part limits them. If the amount of draft affects how the casting is used, state whether it is added to or subtracted from the dimension shown.

How to State Critical Dimensions and Tolerances

Put one general tolerance grade in or near the title block, name the document it comes from, and tolerance individually only the few dimensions that matter.

Use one grade system on a drawing. ISO 8062-3:2023 uses grades DCTG 1 to DCTG 15 for linear dimensions. Older drawings use CT grades from ISO 8062:1994. North American steel work still does, because SFSA Supplement 3 keeps the CT labels for its steel tolerances.

A grade sets a total band that grows with the dimension, so no single ± figure covers a whole part. The band is split evenly about the nominal dimension unless you agree otherwise and state it individually.

Set the grade from what sand molding can hold. For steel sand castings, CT 10 to 12 suits most casting types on long production runs, and CT 11 to 13 on short runs. For iron sand castings in long-series production, the recommended range is DCTG 8 to 12 for machine and shell molding and DCTG 11 to 14 for hand molding, and complex castings take one grade coarser.

A tighter tolerance is possible by agreement. The foundry may need gaging, grinding or pressing to reach it, so ask for that step to be priced.

Call the critical dimensions out individually, using your normal dimensioning and geometric tolerancing standard. Note any parallelism, concentricity, perpendicularity or minimum wall section you need. The general grade does not cover cylindricity or angular dimensions, so these need their own tolerances.

Mark the datum points on the drawing, and use the same ones for the foundry, the machinist and your inspector.

How to Specify the Material

Name a recognized specification and a grade.

You can tighten an ASTM requirement and still get castings certified to that specification. If you relax a requirement, the castings cannot be certified to it. Add only what the design needs.

When the Grade Is Decided

Write the specification, the grade and any class together, then add the common-requirements specification if you want one of its supplements.

  • Carbon steel: “ASTM A216 Grade WCB” or “ASTM A27 Grade 60-30 Class 1”. A27 requires the purchaser to state both grade and class.
  • Ductile iron: “ASTM A536 Grade 65-45-12”.
  • Gray iron: “ASTM A48 Class 30”.

The common-requirements specifications are A781 for steel, A703 for steel pressure-containing parts such as A216 WCB, and A834 for iron. Their supplementary requirements cover added testing and inspection, and each applies only when the order names it individually.

When the Alloy Is Still Open

Send the properties the part needs and its service conditions, then ask the foundry to propose a grade. List the mechanical, physical, chemical or dimensional properties, and leave out the factors that produce them.

If you have a candidate in mind, ask for a price on it and on the foundry’s alternative.

Which Test Bar to Name

Name the bar the material specification uses, and give the controlling wall section. A test bar qualifies the metal in the heat or lot. It does not tell you the properties in the casting.

  • Gray iron: A48 classes rest on separately cast bars, lettered S, A, B or C by the controlling wall section. Give that thickness so the letter can be set from A48.
  • Ductile iron: A536 uses a 1-inch Y-block or keel block. A395 pressure castings use Y-block coupons.
  • Carbon steel: unless you say otherwise, coupons may be cast on the casting or separately. The usual coupon is the A370 keel block.

A bar cut from the casting sounds like the stricter choice, but such a bar does not carry the ASTM bar values.

For thick-section or safety-critical work that needs casting properties, mark the location on the drawing and agree the required values with the foundry before you order.

Which Heat Treatment Condition to State

State a condition only where the grade leaves a choice. Some grades fix it already:

  • A536 60-40-18: full ferritizing anneal.
  • A536 65-45-12 and 80-55-06: as-cast.
  • A536 100-70-03 and 120-90-02: quench and temper, normalize and temper, or an isothermal treatment.
  • A27 Grade U-60-30: not heat treated.

A216 castings may be annealed, normalized, or normalized and tempered. Other A27 grades, apart from N-1, may be fully annealed, normalized, normalized and tempered, or quenched and tempered. Name the condition if your design depends on one of these.

List any treatment the grade does not include, such as a stress relief, as its own requirement.

Which Quantities to Give

Give the annual requirement, the batch size, the program length and the sample quantity as separate numbers.

  • Annual requirement: broken into a monthly or weekly schedule. A best estimate is acceptable.
  • Batch size: how many castings you will buy at a time.
  • Program length: how long the part will run and when production starts, with anticipated need as well as present need.
  • Sample quantity: a separate count for the run you approve before serial production.

Mark which numbers are firm and which are forecasts. Use numbers throughout, because foundries differ widely on what low, medium and high volume mean.

Which Surfaces to Mark for Machining

Mark every machined surface on the drawing, show the allowance or ask the foundry to propose it, and say who does the machining. This belongs in the first package.

On allowance, either state it in a general note or leave it to the foundry when you send a machine drawing. Settle the machining allowance before the pattern is built.

Say whether the foundry ships rough castings or machined parts. Mark any areas to be hardened after casting.

What to Say About Patterns and Tooling

Say whether patterns and core boxes already exist. If they do, describe their type and condition. If they do not, ask the foundry to price new tooling separately and to describe what it will build.

For existing tooling, send these details:

  • Patterns: number of castings on the pattern, pattern material, and the flask size and process it is rigged for, with photos of the cope and drag halves.
  • Core boxes: box sizes, material and cores per box, with photos open and closed.

For new tooling, ask each foundry to state these points:

  • Pattern material: wood, plastic or metal.
  • Pattern mounting: mounted or loose.
  • Core box: full or half.
  • Ownership: who will own the tooling.

Whether to Name the Casting Process

Usually no. State the tolerance, finish and quantity you need, then ask each foundry which process it is quoting and which tolerance grade that process normally holds for it. Fix the process in writing only when you have a reason, such as a qualified part that must not change method.

Shell molding is generally the most dimensionally capable sand process, followed by no-bake and green sand. In SFSA’s data from 15 steel foundries, those gaps were smaller than the variation between foundries running the same process.

Which Inspection and Test Requirements to State

State every test beyond what the specification already includes, with where it applies, the method and the acceptance level. Under A536, hardness, chemical composition, microstructure, pressure tightness, radiographic soundness and magnetic particle inspection bind only when the order names them.

Base each test on service need.

Nondestructive Testing

For each NDT method you require, state the areas covered, the test specification and the acceptance level. Mark the areas on the drawing as well as in the RFQ. A complete requirement reads like this: “Radiograph the marked areas per ASTM E94, acceptance per ASTM E186 severity level 2.”

ASTM’s reference radiographs set no pass level by themselves, so agree with the foundry which discontinuity classes and levels apply.

Name the standard that fits the metal and the section:

  • Radiography, steel: E446 up to 2 in (50.8 mm), E186 from 2 to 4 1/2 in (50.8 to 114 mm).
  • Radiography, iron: E802 for gray iron up to 4 1/2 in (114 mm), E689 for ductile iron, used with the steel reference radiographs.
  • Magnetic particle: E709 for the method, E125 for comparison photographs on ferrous castings.
  • Liquid penetrant: E165.
  • Ultrasonic: A609, for heat-treated carbon, low-alloy and martensitic stainless steel castings. It does not cover iron.

Mechanical and Hardness Testing

Name the specification, then add only what it leaves out. A48 and A536 call for one tension test per lot, and steel pressure castings under A703 call for one per heat. If you want more frequent tests, order them as a supplementary requirement.

A48 and A536 list no hardness value for any grade, so state the Brinell range and the surface it is read on. If you need a hardness check on a casting, specify a pad in a location that suits both the foundry and your inspector. If you need impact testing, state the type and the results required.

Pressure Testing

State whether the casting is pressure tested and give the test medium, pressure and hold time. Say who runs the test and at which stage.

A395 and A703 build the test in and run it after machining. If the foundry ships unmachined castings, the test falls to whoever machines them, unless the RFQ says otherwise. For valve bodies, name MSS SP-61.

Which Documents and Certifications to Request

Request chemistry and mechanical test certification, a test report, a first-sample layout, and PPAP if your program requires it. List each one by name, because the foundry supplies only what the order asks for.

  • Chemistry and mechanical test certification: request them separately if you need both.
  • Test report: for each test ordered, require the heat or lot number, chemistry, bar results, hardness readings, NDT results with the acceptance level applied, and the dimensional report.
  • First-sample layout: a full layout of the sample casting confirms that every machined surface has enough stock.
  • PPAP: name it if your program requires it.

If your company uses the EN 10204 types, name the type.

If the part goes into a federally funded infrastructure project under Buy America rules, say so in the RFQ. For EPA programs, the manufacturer provides a self-certification letter specific to the product and the project.

How to State Surface Finish and Coating

Name a comparator standard and acceptance level for each as-cast surface that matters, and mark those surfaces on the drawing. State any coating with its specification on both the drawing and the order.

Avoid Ra as the acceptance basis on an as-cast surface. Cast surfaces lack the regular pattern of machined ones, so visual and tactile comparators are preferred. Ra stays normal on machined faces.

As a rough guide, green sand and cold-setting molds on small to medium castings run around SCRATA A1 to A3, or about 12.5 µm Ra (490 µin).

Pick the standard by casting type:

  • Steel castings: ASTM A802, stating category numbers and levels.
  • Steel or iron castings: ISO 11971, using SCRATA comparators.
  • Valves, flanges, fittings and other piping components: MSS SP-55, whose 2025 edition added iron castings.

For each requirement, give the areas to check, the number of castings to check, the acceptance level and any discontinuity types you will not accept. Different surfaces of one casting can carry different levels. Keep finish requirements to the surfaces whose function needs them.

Leave out qualitative notes such as “free of fins, cracks and sand”.

What to Tell the Foundry About the Application

Tell the foundry what the part does, its service conditions, and whether it is new or replaces an existing part.

For a replacement, say how the old part failed, and give what you know on these points:

  • Specification: whether the casting met it.
  • Load: whether service loads exceeded the design.
  • Abuse: whether the part was misused.

Which Delivery Details to Include

Give the ship-to address, the required date and what that date means, the delivery term with a named place, and any special packaging.

  • Date: say whether it means ready for inspection, ready to ship or delivered.
  • Partial shipments: say whether you accept them.
  • Delivery term: within the U.S., name the place, as in “F.O.B. place of shipment” or “F.O.B. place of destination”. Across a border, use an Incoterms rule with its version and named place. Avoid a bare “FOB”.
  • Packaging: state special pallets, boxes and rust protection.
  • Paperwork: state label, invoice and shipping document requirements.

For imports into the United States, all wood packaging must be ISPM 15 compliant. USDA APHIS tells importers to put this in the contract, so put it in the RFQ too.

How to Ask for a Quote You Can Compare

Ask every foundry to price the same casting condition and to set out the items below in the same way. Tell them whether the request is budgetary or active, and give a due date that leaves time.

  • Casting condition: state what the piece price covers, such as raw, heat treated or machined, with price breaks at your quantities.
  • Exceptions: require every exception to the drawing, specifications and processing to be listed.
  • Tooling: priced separately, with a description of what it is.
  • Capability: the process, the tolerance grade and the finish allowances the price assumes.
  • Added costs: testing, certification, packaging and freight priced separately, with any subcontracted machining or painting identified.
  • Validity date: a written date the price holds until.
  • Metal surcharge: the base price, the index, the formula and how often it is reviewed.

Ask for the validity date and the surcharge basis together. Many U.S. foundries set a base price and apply a per-pound surcharge that moves monthly, so a valid quote can still change on the invoice.