What Causes Hard Spots in Gray Iron Castings
Hard spots in gray iron castings are usually caused by iron that freezes as iron carbide instead of graphite. That
Hard spots in gray iron castings are usually caused by iron that freezes as iron carbide instead of graphite. That
Read a mill test report for iron castings against the ASTM grade on your purchase order, block by block: header,
Choose a gray iron supplier on how well it controls the iron itself and how it proves the result against
Moving a part from gray iron to ductile iron leaves the machining stock and tolerance grades where they were, but
The European equivalent of ASTM A48 Class 30 gray iron is EN-GJL-200 under EN 1561, and the older German equivalent
Gray iron fits a pump casing on clean water at ordinary pressure; higher pressure, freezing, abrasive slurry and corrosive liquids
For most gearbox and bearing housings, ASTM A48 Class 30 is the better callout; move to Class 40 only when
A first order of gray iron sand castings on a new pattern takes longest, because the pattern build alone ran
Cast iron pump castings leak on pressure test when porosity in the sections that freeze last joins into a channel
Most cast iron parts belong in a sand mold: green sand for long runs of parts under a few hundred
An iron casting is proved on five things: chemical composition, mechanical properties from a test bar, microstructure, internal and surface
Cast iron comes in five types — gray, ductile, compacted graphite, white and malleable — and what separates them is
A spark test, a chisel cut or a fresh fracture places an unmarked part on one side or the other,
There is no single ASTM standard for cast iron. ASTM publishes a family of separate iron-casting specifications under Committee A04,
Choose cast steel when the part must take impact, bending or internal pressure and yield before it breaks; choose cast
The difference between ductile iron and gray iron is the shape of the graphite: ductile iron carries it as spheroids,